DIEVAR imported steel nitriding and carbonitriding
Nitriding and carbonitriding to increase the hardness of the mold surface, improve its wear resistance, corrosion resistance and prevent premature cracking.DIEVAR nitriding and carbonitriding can be performed in ion furnaces, controlled atmosphere furnaces and salt furnaces flow. The nitriding temperature should be {{0}} degree below the previous tempering temperature. In addition, inadequate nitriding can also have undesirable consequences, such as reduced mold core hardness and strength and a change in mold scale utility. During nitriding and carbonitriding, a layer of brittle compound known as a white layer may appear. The white layer cracks or breaks and cracks. DIEVAR can achieve an agreed surface hardness of 1000 HV0.2 after gas nitriding at 510 degree* or ion nitriding at 480 degree. Normal ion nitriding is recommended, as the nitrogen concentration is easier to control. Tightly controlled gas nitriding can do the same at material cooling temperatures.
Main chemical composition.
C:0.39,.
CR:4.8.
Mo:2.4.
V:0.5.
If:0,24.
Function.
Samples were taken from the centers of imported 61 615 degree for 2 hours each dievar hardness at the material quenching temperature 45±1 HRC.
Applications.
Zinc, magnesium, aluminum and titanium alloy die casting dies, hot extrusion dies (such as: die core bushings, ejector bars, bearing blocks, etc.), hot forging dies, etc.
DIEVAR Factory Condition: HB160
(5) Tempered
Choose a suitable tempering temperature based on the required hardness. Temper die casting dies at least 3 times and hot forging and extrusion dies twice. After each tempering should be cooled to room temperature, each tempering at least 2 hours of insulation. 500 ~ 550 degree tempering to avoid the brittleness of tempering.
(6) Hardening and rescaling after tempering
During the quenching and tempering process, the mold is distorted and deformed by the arrangement of thermal and variable stresses. Failure to retain sufficient mold headroom will slow mold hardening during the heat treatment process. To guess the large mold deformation in normal hardening, it is generally recommended that stress relief be performed between roughing and semi-finishing processes. After stress relief, it is advised that DIEVAR molds reserve at least 0.3 during quenching, % of machining and quantity to meet the mold deformation tolerance.